Display panel and fabricating method thereof
11762239 · 2023-09-19
Assignee
Inventors
Cpc classification
C23C18/1204
CHEMISTRY; METALLURGY
G02F1/1368
PHYSICS
G02F1/133614
PHYSICS
C09D11/50
CHEMISTRY; METALLURGY
C23C18/1283
CHEMISTRY; METALLURGY
C23C18/1295
CHEMISTRY; METALLURGY
International classification
G02F1/1335
PHYSICS
C09D11/50
CHEMISTRY; METALLURGY
C23C18/12
CHEMISTRY; METALLURGY
Abstract
A display panel and a fabricating method thereof are provided. The fabricating method of the display panel has steps of: providing a substrate; forming a light conversion layer on the substrate, wherein material of the light conversion layer has a perovskite structural material with a chemical formula of ABX.sub.3, wherein A represents an inorganic element, B represents an inorganic element, and X represents a halogen; performing a patterning step on the light conversion layer by an antisolvent method, wherein the light conversion layer forms a plurality of light conversion patterns; and forming a pixel layer on the light conversion layer, wherein the pixel layer has a plurality of pixel units, and the plurality of pixel units are respectively aligned with the plurality of light conversion patterns. The fabricating method can reduce a dark state brightness of the display panel, thereby improving contrast of the display panel.
Claims
1. A fabricating method of a display panel, comprising steps of: providing a substrate; forming a light conversion layer on the substrate, wherein material of the light conversion layer comprises a perovskite structural material with a chemical formula of ABX.sub.3, wherein A represents an inorganic element, B represents an inorganic element, and X represents a halogen, wherein the step of forming the light conversion layer comprises: coating a perovskite precursor solution on the substrate; and performing a low-temperature vacuum drying treatment with a treating temperature ranged between 90 and 130° C. on the perovskite precursor solution to form the light conversion layer on the substrate; performing a patterning step on the light conversion layer by an antisolvent method, wherein the light conversion layer forms a plurality of light conversion patterns, and an antisolvent of the antisolvent method comprises at least one of chlorobenzene and toluene; and forming a pixel layer on the light conversion layer, wherein the pixel layer comprises a plurality of pixel units, and the plurality of pixel units are respectively aligned with the plurality of light conversion patterns.
2. The fabricating method of the display panel according to claim 1, wherein a treating time of the low-temperature vacuum drying treatment is between 5 to 15 minutes.
3. The fabricating method of the display panel according to claim 1, wherein the patterning step comprises steps of: defining positions of the plurality of light conversion patterns of the light conversion layer; inkjet printing the antisolvent at the positions of the plurality of light conversion patterns; and performing a low-temperature vacuum drying process with a treating temperature ranged between 90 and 130° C. on the anti-solvent to form the plurality of light conversion patterns.
4. The fabricating method of the display panel according to claim 3, wherein a treating time of the low-temperature vacuum drying process on the anti-solvent is between 5 to 15 minutes.
5. The fabricating method of the display panel according to claim 1, wherein the A comprises at least one of sodium, potassium, cesium, and barium.
6. The fabricating method of the display panel according to claim 1, wherein the B comprises at least one of copper, nickel, cobalt, iron, manganese, chromium, cadmium, tin, and lead.
7. The fabricating method of the display panel according to claim 1, wherein the X comprises at least one of chlorine, bromine, and iodine.
8. A fabricating method of a display panel, comprising steps of: providing a substrate; forming a light conversion layer on the substrate, wherein material of the light conversion layer comprises a perovskite structural material with a chemical formula of ABX.sub.3, wherein A represents an inorganic element, B represents an inorganic element, and X represents a halogen; performing a patterning step on the light conversion layer by an antisolvent method, wherein the light conversion layer forms a plurality of light conversion patterns; and forming a pixel layer on the light conversion layer, wherein the pixel layer comprises a plurality of pixel units, and the plurality of pixel units are respectively aligned with the plurality of light conversion patterns.
9. The fabricating method of the display panel according to claim 8, wherein the step of forming the light conversion layer comprises steps of: coating a perovskite precursor solution on the substrate; and performing a low-temperature vacuum drying treatment with a treating temperature ranged between 90 and 130° C. on the perovskite precursor solution to form the light conversion layer on the substrate.
10. The fabricating method of the display panel according to claim 9, wherein a treating time of the low-temperature vacuum drying treatment is between 5 to 15 minutes.
11. The fabricating method of the display panel according to claim 8, wherein an antisolvent of the antisolvent method comprises at least one of chlorobenzene and toluene.
12. The fabricating method of the display panel according to claim 8, wherein the patterning step comprises steps of: defining positions of the plurality of light conversion patterns of the light conversion layer; inkjet printing the antisolvent at the positions of the plurality of light conversion patterns; and performing a low-temperature vacuum drying process with a treating temperature ranged between 90 and 130° C. on the anti-solvent to form the plurality of light conversion patterns.
13. The fabricating method of the display panel according to claim 12, wherein a treating time of the low-temperature vacuum drying process on the anti-solvent is between 5 to 15 minutes.
14. The fabricating method of the display panel according to claim 8, wherein the A comprises at least one of sodium, potassium, cesium, and barium.
15. The fabricating method of the display panel according to claim 8, wherein the B comprises at least one of copper, nickel, cobalt, iron, manganese, chromium, cadmium, tin, and lead.
16. The fabricating method of the display panel according to claim 8, wherein the X comprises at least one of chlorine, bromine, and iodine.
Description
BRIEF DESCRIPTION OF THE SEVERAL VIEWS OF THE DRAWINGS
(1)
(2)
DESCRIPTION OF SPECIFIC EMBODIMENTS OF THE INVENTION
(3) Following description of the various embodiments is provided to illustrate the specific embodiments of the present disclosure. Furthermore, directional terms mentioned in the present disclosure, such as upper, lower, top, bottom, front, rear, left, right, inner, outer, side, surrounding, central, horizontal, horizontal, vertical, longitudinal, axial, radial, an uppermost layer or a lowermost layer, etc., only refer to a direction of the accompanying figures. Therefore, the used directional terms are used to describe and understand the present disclosure, but the present disclosure is not limited thereto.
(4) Referring to
(5) In an embodiment of the present disclosure, the fabricating method 10 of the display panel has a step 11 of: providing a substrate. In step 11, the substrate can be used to support a structure required in the display panel, such as a light conversion layer and a pixel layer described later. In one embodiment, the substrate can also be used to support other components in the display panel, such as a diffusion sheet, a brightness enhancement sheet, a polarizer, or a liquid crystal layer. In another embodiment, the substrate includes a flexible substrate, a transparent substrate, or a flexible transparent substrate.
(6) In an embodiment of the present disclosure, the fabricating method 10 of the display panel has a step 12 of: forming a light conversion layer on the substrate, wherein material of the light conversion layer comprises a perovskite structural material with a chemical formula of ABX.sub.3, wherein A represents an inorganic element, B represents an inorganic element, and X represents a halogen. In step 12, the light conversion layer can be formed on the substrate by, for example, coating or deposition. In an embodiment, a perovskite precursor solution is coated on the substrate, and then a low-temperature vacuum drying treatment is performed on the perovskite precursor solution to form the light conversion layer on the substrate. In an example, a treating temperature of the low-temperature vacuum drying treatment is between 90 and 130° C. (for example, 100° C., 110° C., or 120° C.) for 5 to 15 minutes (for example, 6, 7, 8, 10, 12, 13, or 14 minutes). In an embodiment, the A comprises at least one of sodium, potassium, cesium, and barium. In another embodiment, the B includes at least one of copper, nickel, cobalt, iron, manganese, chromium, cadmium, tin, and lead. In yet another embodiment, the X includes at least one of chlorine, bromine, and iodine.
(7) In an embodiment of the present disclosure, the fabricating method 10 of the display panel has a step 13 of: performing a patterning step on the light conversion layer by an antisolvent method, wherein the light conversion layer forms a plurality of light conversion patterns. In step 13, positions of the plurality of light conversion patterns are mainly determined by an anti-solvent method. More specifically, only the light conversion layer treated by the antisolvent method can achieve effective light emission, and other untreated parts can be used to absorb light. In an embodiment, the positions of the plurality of light conversion patterns of the light conversion layer are first defined. Thereafter, an antisolvent is inkjet printed on the positions of the plurality of light conversion patterns. Finally, a low-temperature vacuum drying treatment is performed on the anti-solvent to form the plurality of light conversion patterns. In an example, a treating temperature of the low-temperature vacuum drying treatment is between 90 and 130° C. (for example, 100° C., 110° C., or 120° C.) for 5 to 15 minutes (for example, 6, 7, 8, 10, 12, 13, or 14 minutes).
(8) In an embodiment of the present disclosure, the fabricating method 10 of the display panel has a step 14 of: forming a pixel layer on the light conversion layer, wherein the pixel layer comprises a plurality of pixel units, and the plurality of pixel units are respectively aligned with the plurality of light conversion patterns. In step 14, the pixel layer can be formed using a known process of a pixel layer, for example. In an embodiment, the plurality of pixel units can be used to display red, green, or blue, for example.
(9) From above, because the plurality of pixel units are aligned with the plurality of light conversion patterns, respectively, only the light passing through the light conversion patterns can reach the positions of the plurality of pixel units to display colors, and the light that does not pass through the light conversion patterns will be absorbed. Therefore, the display panel fabricated by the fabricating method of the display panel according to an embodiment of the present disclosure can prevent or reduce light from passing through a non-pixel effective light emitting area, and the dark state brightness of the display panel can be reduced, which further improves the contrast of the display panel.
(10) Referring to
(11) In an embodiment, the display panel 20 can further comprises a light emitting layer (for example, including a blue LED and potassium fluorosilicate fluorescent powder (KSF fluorescent powder)) 24, a diffusion sheet 25, a brightness enhancement sheet (BEF) 26, a dual brightness enhancement sheet (DBEF) 27, a lower polarizer 28, a TFT array and color filter substrate 29 and an upper polarizer 30, wherein the pixel layer 23 is disposed in the TFT array and color filter substrate 28.
(12) In an embodiment, the display panel 20 of the present disclosure can be fabricated by the fabricating method 10 of the display panel of the present disclosure, for example.
(13) The present disclosure has been described in relative embodiments described above, but the above embodiments are merely examples for implementing the present disclosure. It is noted that the disclosed embodiments do not limit the scope of the disclosure. On the contrary, modifications and equal settings included in the spirit and scope of the claims are all included in the scope of the present disclosure.